サポート

Question about special ink

Although he wants to perform Tijimi printing ...

Tijimi pattern does not generate Tijimi printing only in Tijimi ink (TJN Medium). They are the patent products of our company which wrinkles generate by the set of a Tijimi lamp and Tijimi ink. First of all, please tell us the purchase of a lamp to our company operating charge.

Although he wants to enlarge the pattern of Tijimi ...

It is in two enlarging a Tijimi pattern.

  1. Please thicken film thickness of ink.
  2. Please make a Tijimi lamp output low.

Although he wants to make the pattern of Tijimi small ...

Be in two making a Tijimi pattern small.

  1. Please make film thickness of ink thin. It will become free overcoat if too thin.
  2. Please make a Tijimi lamp output high. It hardens, before Tijimi will occur, if too high, and a Tijimi pattern does not occur.

Although he wants to carry out Tijimi printing to Processing PP etc. ...

Since Tijimi ink (TJN Medium) has few materials to stick, to the material which is not stuck, please print SG740 etc. as a binder and perform Tijimi printing from on the.

Please let me know the specular surface ink stuck to hard court acrylics.

A. Please use specular surface ink 600HR for hard court acrylics.

Can mixing colors of the specular surface ink be carried out?

A. As for specular surface ink NO.3 series, it is possible for there to be a standard color of nine colors and it to carry out mixing colors in addition to silver. The standard color is as follows.

  1. 208 process yellow
  2. 209 yellow
  3. 304 process green
  4. 456 process blue
  5. 498 process violet
  6. 513 permanent red
  7. 538 process red
  8. 580 magentas
  9. 765 process black

Although he wants to drop specular surface nature ...

the case where specular surface nature is dropped on blunt gloss like platinum -- a mat agent, the usual silver powder, and the coat for specular surfaces -- clear may be mixed Even our company mixing-colors staff needs to consult.

Is a half mirror reproducible by printing?

There is a half mirror as penetrable good specular surface ink like vapor deposition.

Which series is the ink with the most sufficient growth?

Although SG410 and RUX are extended well, there is a demerit that hardening is slow. It is used as insert molding ink of a urethane sheet.

Is there any binder which puts insert molding ink and insertion resin together?

We recommend you JT20 and JT25. It uses properly according to the kind of insert molding ink, and the kind of insertion resin.

Although insert molding ink will melt with the heat of insertion resin ...

If insert molding ink has not hardened completely, it may melt with heat. After printing / dryness, please pour insertion resin after placing about one day.